ECSS Structures — COSPE with Homogeneous Non-Metallic Liner (space-systems/ecss/cospe-nonmetallic-liner)
Use when the task is the structural assessment of a composite
overwrapped pressure vessel with a homogeneous non-metallic liner
under ECSS-E-ST-32C clause 4.6.3 — checking that liner material
family, proof and burst margins, liner strain at proof, overwrap
fiber volume fraction, and environmental degradation factors are
all within acceptable bounds before the vessel is considered
structurally compliant.
Domain quick reference
ECSS-E-ST-32C clause 4.6.3 covers COSPE vessels whose liner is a
homogeneous non-metallic material (polymer, elastomer, thermoplastic,
thermoset, or fluoropolymer). The liner carries the leak-tight
pressure boundary; the composite overwrap provides the primary
structural load path. The two must be strain-compatible at proof
pressure: the liner strain at proof must not exceed its own allowable
strain.
Proof and burst pressure factors are the ratio of proof or burst
pressure to the maximum allowable working pressure (MAWP). The
minimum proof factor is 1.1 and the minimum burst factor is 1.5.
Environmental degradation (moisture absorption, thermal cycling,
UV, chemical exposure) reduces effective burst strength; a
degradation factor (0 < f ≤ 1.0) is multiplied against the burst
pressure before the effective burst factor is computed.
The overwrap fiber volume fraction (FVF) must lie within defined
bounds (0.50 to 0.70 inclusive). A value below the lower bound
indicates insufficient fiber density; a value above the upper bound
indicates resin starvation and elevated void content. Both
conditions are structural risks and are flagged independently.
A vessel is not structurally compliant until every margin check
passes: proof factor, effective burst factor, liner strain
compatibility, and FVF.
Workflow
- Confirm the liner material family is a recognized non-metallic
category. Reject any unrecognized liner material before the rest of
the assessment proceeds.
- Check the proof pressure factor: divide proof pressure by MAWP and
verify the result is at least 1.1. Flag a shortfall.
- Apply the environmental degradation factor to the burst pressure to
obtain the effective burst strength. Divide by MAWP and verify the
effective factor is at least 1.5. Flag a shortfall.
- Check liner strain compatibility: verify the liner strain at proof
pressure does not exceed the liner allowable strain. Flag an
exceedance.
- Check the overwrap fiber volume fraction: verify it lies between
0.50 and 0.70 inclusive. Flag values below the lower bound and
above the upper bound separately.
- Aggregate all findings. The vessel is compliant only when every
finding list is empty.
Pitfalls
- Omitting the degradation factor and using raw burst pressure to
compute the burst factor — environmental exposure reduces effective
burst strength; using the undegraded value overstates margin and
may allow a non-compliant vessel to appear compliant.
- Treating a missing or unrecognized liner material entry as a pass —
an unrecognized liner type is outside the validated range and must
be rejected before any margin check runs.
- Using MAWP as zero or negative — all factor calculations divide by
MAWP; a zero or negative MAWP is a data error and must be caught
before computation proceeds.
- Checking FVF against only one bound — both a low FVF (fiber
starvation) and a high FVF (resin starvation with elevated void
content) are structural risks and both bounds must be verified.
- Applying the degradation factor greater than 1.0 — a degradation
factor above 1.0 would imply the vessel gains strength from
environmental exposure, which is physically inadmissible; a value
outside (0, 1.0] must be rejected.
Behavior contract (gate 3)
The liner categorization, proof factor, burst factor, liner strain
compatibility, and FVF checks are exercised by the gate 3 contract
test: scripts/test_cospe_nonmetallic_liner.py against
scripts/cospe_nonmetallic_liner_logic.py (stdlib unittest, offline).
Run:
python3 scripts/test_cospe_nonmetallic_liner.py
Compliance
- ECSS standards are freely downloadable (ESA); cite the source and
paraphrase per standards-map.yaml.
- compliance: STANDARDS-REF, gated: false.
1---2name: cospe-nonmetallic-liner3description: "Use when assess the structural integrity of a composite overwrapped pressure vessel with a homogeneous non-metallic liner per ECSS-E-ST-32C clause 4.6.3: categorize the liner material family, verify the proof pressure and burst pressure factors against the maximum allowable working pressure, check liner strain at proof pressure against the liner allowable strain, validate the overwrap fiber volume fraction, and apply environmental degradation to the effective burst margin. A vessel assessment is not compliant until all margin checks pass. Trigger: ecss, e-st-32-structures-scope, cospe, composite-overwrapped-pressure-vessel, nonmetallic-liner, burst-factor, proof-factor, strain-compatibility."4license: Apache-2.05compliance: STANDARDS-REF6standards:7 - id: ecss8 reference-only: true9gated: false10domain: space-systems11pack: space-systems12compatibility: "agentskills.io SKILL.md; any SKILL.md host (Claude Code, Hermes, OpenClaw)"13metadata:14 source: https://skillmd.com/skills/ashfordeou/cospe-nonmetallic-liner15 domain: space-systems16 subdomain: ecss17 tags: [ecss, e-st-32-structures-scope, cospe, composite-overwrapped-pressure-vessel, nonmetallic-liner, burst-factor, proof-factor, strain-compatibility]18 version: 0.1.019 author: Aero Agent Skills20---2122# ECSS Structures — COSPE with Homogeneous Non-Metallic Liner (space-systems/ecss/cospe-nonmetallic-liner)2324Use when the task is the structural assessment of a composite25overwrapped pressure vessel with a homogeneous non-metallic liner26under ECSS-E-ST-32C clause 4.6.3 — checking that liner material27family, proof and burst margins, liner strain at proof, overwrap28fiber volume fraction, and environmental degradation factors are29all within acceptable bounds before the vessel is considered30structurally compliant.3132## Domain quick reference3334- ECSS-E-ST-32C clause 4.6.3 covers COSPE vessels whose liner is a35 homogeneous non-metallic material (polymer, elastomer, thermoplastic,36 thermoset, or fluoropolymer). The liner carries the leak-tight37 pressure boundary; the composite overwrap provides the primary38 structural load path. The two must be strain-compatible at proof39 pressure: the liner strain at proof must not exceed its own allowable40 strain.4142- Proof and burst pressure factors are the ratio of proof or burst43 pressure to the maximum allowable working pressure (MAWP). The44 minimum proof factor is 1.1 and the minimum burst factor is 1.5.45 Environmental degradation (moisture absorption, thermal cycling,46 UV, chemical exposure) reduces effective burst strength; a47 degradation factor (0 < f ≤ 1.0) is multiplied against the burst48 pressure before the effective burst factor is computed.4950- The overwrap fiber volume fraction (FVF) must lie within defined51 bounds (0.50 to 0.70 inclusive). A value below the lower bound52 indicates insufficient fiber density; a value above the upper bound53 indicates resin starvation and elevated void content. Both54 conditions are structural risks and are flagged independently.5556- A vessel is not structurally compliant until every margin check57 passes: proof factor, effective burst factor, liner strain58 compatibility, and FVF.5960## Workflow61621. Confirm the liner material family is a recognized non-metallic63 category. Reject any unrecognized liner material before the rest of64 the assessment proceeds.652. Check the proof pressure factor: divide proof pressure by MAWP and66 verify the result is at least 1.1. Flag a shortfall.673. Apply the environmental degradation factor to the burst pressure to68 obtain the effective burst strength. Divide by MAWP and verify the69 effective factor is at least 1.5. Flag a shortfall.704. Check liner strain compatibility: verify the liner strain at proof71 pressure does not exceed the liner allowable strain. Flag an72 exceedance.735. Check the overwrap fiber volume fraction: verify it lies between74 0.50 and 0.70 inclusive. Flag values below the lower bound and75 above the upper bound separately.766. Aggregate all findings. The vessel is compliant only when every77 finding list is empty.7879## Pitfalls8081- Omitting the degradation factor and using raw burst pressure to82 compute the burst factor — environmental exposure reduces effective83 burst strength; using the undegraded value overstates margin and84 may allow a non-compliant vessel to appear compliant.85- Treating a missing or unrecognized liner material entry as a pass —86 an unrecognized liner type is outside the validated range and must87 be rejected before any margin check runs.88- Using MAWP as zero or negative — all factor calculations divide by89 MAWP; a zero or negative MAWP is a data error and must be caught90 before computation proceeds.91- Checking FVF against only one bound — both a low FVF (fiber92 starvation) and a high FVF (resin starvation with elevated void93 content) are structural risks and both bounds must be verified.94- Applying the degradation factor greater than 1.0 — a degradation95 factor above 1.0 would imply the vessel gains strength from96 environmental exposure, which is physically inadmissible; a value97 outside (0, 1.0] must be rejected.9899## Behavior contract (gate 3)100101The liner categorization, proof factor, burst factor, liner strain102compatibility, and FVF checks are exercised by the gate 3 contract103test: scripts/test_cospe_nonmetallic_liner.py against104scripts/cospe_nonmetallic_liner_logic.py (stdlib unittest, offline).105Run:106python3 scripts/test_cospe_nonmetallic_liner.py107108## Compliance109110- ECSS standards are freely downloadable (ESA); cite the source and111 paraphrase per standards-map.yaml.112- compliance: STANDARDS-REF, gated: false.