ECSS Structures — Composite Overwrap Inspection (space-systems/ecss/overwrap-inspection)
Use when the task is to assess the integrity of a composite overwrap on a
spacecraft pressure vessel or structure per ECSS-E-ST-32C clause 5.7 —
selecting the non-destructive testing (NDT) method for each detected anomaly,
applying visual damage tolerance (VDT) criteria to surface findings, and
producing an inspection verdict.
Domain quick reference
- Clause 5.7 requires that composite overwraps on pressure vessels and
structural elements be inspected using methods suited to the anomaly type
and overwrap material. Accepted overwrap materials are carbon-fibre
reinforced polymer (CFRP), glass-fibre reinforced polymer (GFRP), and
aramid-fibre composites; the NDT method matrix is material-specific.
- Anomaly types addressed: voids (internal pores from fabrication), delaminations
(inter-ply separations), surface scratches, fibre breakage, and inclusions
(foreign matter entrapped during lay-up). Each type is categorized into one
of three severity bands — acceptable (no action required), monitor (re-inspect
at next opportunity), or rejectable (remove from service pending disposition) —
based on a size threshold specific to that type.
- NDT methods in scope: ultrasonic testing (UT), radiography (X-ray), active
thermography (AT), visual inspection (VI), and acoustic emission (AE). Method
selection is driven by the combination of defect type and overwrap material;
surface anomalies are evaluated by VDT first, before committing to volumetric
NDT.
- Inspection coverage is a mandatory metric: the ratio of inspected area to
total overwrap area must reach or exceed 95 % before an inspection can yield
a pass or fail verdict; below that threshold the result is "incomplete" and
additional coverage is required.
Workflow
- Identify every detected anomaly on the overwrap and record its type and
maximum linear dimension in millimetres. Reject any anomaly whose type is
not in the recognized set before it enters the sizing assessment; an
unrecognized anomaly type requires disposition by the responsible structures
engineer before proceeding.
- For each surface anomaly (scratch, visible fibre breakage), apply visual
damage tolerance: compare against the VDT acceptance limits for the
overwrap material. Anomalies within VDT limits are acceptable without
further volumetric NDT; anomalies beyond the VDT limit escalate to
volumetric NDT in the next step.
- For each volumetric or escalated anomaly, consult the NDT method matrix
(defect type × overwrap material) to select the recommended method or
methods. Document the method chosen and the rationale when deviating from
the matrix recommendation.
- Categorize each anomaly using the size-based thresholds for its type:
within the acceptable limit → acceptable; between acceptable and monitor
limits → monitor; above the monitor limit → rejectable. Aggregate the
worst category across all anomalies on the same overwrap.
- Compute inspection coverage as (inspected area / total overwrap area) × 100.
If coverage is below 95 %, return an "incomplete" verdict regardless of
anomaly findings and request additional inspection to close the gap.
- Determine the overall inspection verdict: pass (all anomalies acceptable,
coverage adequate), conditional-pass (worst category is monitor, coverage
adequate), fail (any rejectable anomaly, coverage adequate), or incomplete
(coverage below threshold). A fail requires a formal disposition record
before the component may be used.
Pitfalls
- Applying volumetric NDT to every finding without first screening surface
anomalies by VDT — VDT is the first gate for surface indications and avoids
unnecessary intrusive inspection of acceptable scratches or marks.
- Using an NDT method from outside the recommended matrix for the overwrap
material without documented justification — method mismatch can leave
characteristic defect types undetected in that material system.
- Treating an incomplete coverage result as a pass because no rejectable
anomaly was found in the inspected region — uninspected area carries unknown
risk, so a coverage shortfall is itself a non-conformance.
- Combining anomalies of different types into a single worst-size figure and
applying a single threshold — each defect type has its own acceptance limits
and must be assessed independently before aggregating the category verdict.
- Failing to escalate an unrecognized anomaly type to the structures engineer
and instead applying the nearest known type's limits — limits are specific
to each anomaly morphology and are not interchangeable.
Behavior contract (gate 3)
The NDT method selection, defect categorization, coverage assessment, and
inspection result logic are exercised by the gate 3 contract test:
scripts/test_overwrap_inspection.py against scripts/overwrap_inspection_logic.py
(stdlib unittest, offline). Run:
python3 scripts/test_overwrap_inspection.py
Compliance
- ECSS standards are freely downloadable (ESA); cite the source and
paraphrase per standards-map.yaml.
- compliance: STANDARDS-REF, gated: false.
1---2name: overwrap-inspection3description: "Use when assess composite overwrap integrity per ECSS-E-ST-32C clause4 5.7: select the non-destructive testing method appropriate to the detected anomaly5 type and overwrap material (CFRP, GFRP, aramid), evaluate inspection coverage against6 the required threshold, categorize each defect as acceptable, monitor, or rejectable7 using established size criteria, and determine the overall inspection outcome (pass,8 conditional-pass, fail, or incomplete). Apply visual damage tolerance evaluation9 to surface anomalies before committing to invasive NDT. Trigger: ecss, e-st-32-structures-scope,10 overwrap-inspection, composite-overwrap, ndt, vdt, delamination, void."11license: Apache-2.012compliance: STANDARDS-REF13standards:14 - id: ecss15 reference-only: true16gated: false17domain: space-systems18pack: space-systems19compatibility: "agentskills.io SKILL.md; any SKILL.md host (Claude Code, Hermes, OpenClaw)"20metadata:21 source: https://skillmd.com/skills/ashfordeou/overwrap-inspection22 domain: space-systems23 subdomain: ecss24 tags: [ecss, e-st-32-structures-scope, overwrap-inspection, composite-overwrap, ndt, vdt, delamination, void]25 version: 0.1.026 author: Aero Agent Skills27---2829# ECSS Structures — Composite Overwrap Inspection (space-systems/ecss/overwrap-inspection)3031Use when the task is to assess the integrity of a composite overwrap on a32spacecraft pressure vessel or structure per ECSS-E-ST-32C clause 5.7 —33selecting the non-destructive testing (NDT) method for each detected anomaly,34applying visual damage tolerance (VDT) criteria to surface findings, and35producing an inspection verdict.3637## Domain quick reference3839- Clause 5.7 requires that composite overwraps on pressure vessels and40 structural elements be inspected using methods suited to the anomaly type41 and overwrap material. Accepted overwrap materials are carbon-fibre42 reinforced polymer (CFRP), glass-fibre reinforced polymer (GFRP), and43 aramid-fibre composites; the NDT method matrix is material-specific.44- Anomaly types addressed: voids (internal pores from fabrication), delaminations45 (inter-ply separations), surface scratches, fibre breakage, and inclusions46 (foreign matter entrapped during lay-up). Each type is categorized into one47 of three severity bands — acceptable (no action required), monitor (re-inspect48 at next opportunity), or rejectable (remove from service pending disposition) —49 based on a size threshold specific to that type.50- NDT methods in scope: ultrasonic testing (UT), radiography (X-ray), active51 thermography (AT), visual inspection (VI), and acoustic emission (AE). Method52 selection is driven by the combination of defect type and overwrap material;53 surface anomalies are evaluated by VDT first, before committing to volumetric54 NDT.55- Inspection coverage is a mandatory metric: the ratio of inspected area to56 total overwrap area must reach or exceed 95 % before an inspection can yield57 a pass or fail verdict; below that threshold the result is "incomplete" and58 additional coverage is required.5960## Workflow61621. Identify every detected anomaly on the overwrap and record its type and63 maximum linear dimension in millimetres. Reject any anomaly whose type is64 not in the recognized set before it enters the sizing assessment; an65 unrecognized anomaly type requires disposition by the responsible structures66 engineer before proceeding.672. For each surface anomaly (scratch, visible fibre breakage), apply visual68 damage tolerance: compare against the VDT acceptance limits for the69 overwrap material. Anomalies within VDT limits are acceptable without70 further volumetric NDT; anomalies beyond the VDT limit escalate to71 volumetric NDT in the next step.723. For each volumetric or escalated anomaly, consult the NDT method matrix73 (defect type × overwrap material) to select the recommended method or74 methods. Document the method chosen and the rationale when deviating from75 the matrix recommendation.764. Categorize each anomaly using the size-based thresholds for its type:77 within the acceptable limit → acceptable; between acceptable and monitor78 limits → monitor; above the monitor limit → rejectable. Aggregate the79 worst category across all anomalies on the same overwrap.805. Compute inspection coverage as (inspected area / total overwrap area) × 100.81 If coverage is below 95 %, return an "incomplete" verdict regardless of82 anomaly findings and request additional inspection to close the gap.836. Determine the overall inspection verdict: pass (all anomalies acceptable,84 coverage adequate), conditional-pass (worst category is monitor, coverage85 adequate), fail (any rejectable anomaly, coverage adequate), or incomplete86 (coverage below threshold). A fail requires a formal disposition record87 before the component may be used.8889## Pitfalls9091- Applying volumetric NDT to every finding without first screening surface92 anomalies by VDT — VDT is the first gate for surface indications and avoids93 unnecessary intrusive inspection of acceptable scratches or marks.94- Using an NDT method from outside the recommended matrix for the overwrap95 material without documented justification — method mismatch can leave96 characteristic defect types undetected in that material system.97- Treating an incomplete coverage result as a pass because no rejectable98 anomaly was found in the inspected region — uninspected area carries unknown99 risk, so a coverage shortfall is itself a non-conformance.100- Combining anomalies of different types into a single worst-size figure and101 applying a single threshold — each defect type has its own acceptance limits102 and must be assessed independently before aggregating the category verdict.103- Failing to escalate an unrecognized anomaly type to the structures engineer104 and instead applying the nearest known type's limits — limits are specific105 to each anomaly morphology and are not interchangeable.106107## Behavior contract (gate 3)108109The NDT method selection, defect categorization, coverage assessment, and110inspection result logic are exercised by the gate 3 contract test:111scripts/test_overwrap_inspection.py against scripts/overwrap_inspection_logic.py112(stdlib unittest, offline). Run:113114 python3 scripts/test_overwrap_inspection.py115116## Compliance117118- ECSS standards are freely downloadable (ESA); cite the source and119 paraphrase per standards-map.yaml.120- compliance: STANDARDS-REF, gated: false.